WEM Universal Clay Plaster

Technical Data

Product nameUniversal dry clay plaster,
DIN 18947 – LPM 0/2 f – SII -1.8
Scope of applicationSingle- or multi-layer indoor plaster suitable for plaster-throwing machines or manual application on all sub bases appropriate for rendering. Due to its composition, the plaster is a perfect heating plaster for radiant wall heating systems. It embeds the pipe and conducts the heat from the heating pipe to the wall surface.
Properties

Composition: Milled construction loam, quartz sand, natural fibres
Coating thickness: 5 to 23 mm
Grain group/grain oversize: 0/2 mm
Bulk density class: 1.8
Drying shrinkage: < 2.5 %
Strength class: S II
Compressive resistance: 2.2 N/mm2
Flexural strength: > 0,7 N/mm2
Adhesive strength: ≥ 0.1 N/mm2
Thermal conductivity: 0.91 W/(mK)
Vapour diffusion resistance class: WS III
Material class: B2
Abrasion: 0.1 g

Storage/
storage life
In a dry storage place, the shelf life of the plaster is unlimited.
Coverage25 kg Clay Universal Plaster gives 16.6 litres of rendering mortar.
This quantity is sufficient for a surface of approx. 1.66 m2 with a
coat thickness of 10 mm or for a surface of 0.72 m2 with a coat
thickness of 23 mm (approx. 1.506 kg/m2 per mm application
thickness).
ProcessingAdd 5.4 litres of water to 25 kg of plaster. The sub base must be
clean, free from film-forming separating agents and sufficiently
rough because the clay plaster adheres mechanically. Pre-wetting
is not necessary. Apply the plaster either manually with a trowel or
with a plastering machine. If a single coat is applied, it may have a
thickness between 5 and 23 mm. You can apply multiple coats,
however.
Workability
and drying
The ready-mixed material remains workable for several days if
stored in a closed recipient. You may have to add some more
water before reuse. Operate the wall heating at a supply
temperature of 30 to 45 °C immediately after the application of the
clay plaster to accelerate the drying process. Remove moisture
through cross ventilation or with a dehumidifyer. If you cannot
operate the heating you must use appropriate machinery for drying.
Consider the drying report of the German Association for the
Promotion of Clay Building Materials (DVL).
(www.wall-heating.com/tp).
Finishing

Apply subsequent paint or plaster finishes only after all plaster layers have dried completely.

Apply finish coats in accordance with the clay building rules (Lehmbau-Regeln (3.9)) of the German Association for Building with Earth DVL (Dachverband Lehm e.V.)